MEMSnet Home: MEMS-Talk: "Sharp edge" problem with EPON photoresist
"Sharp edge" problem with EPON photoresist
1998-06-17
Hui Tang
"Sharp edge" problem with EPON photoresist
Hui Tang
1998-06-17
Dear MEMS experts,

    I am making some very thick patterns (thickness: ~0.7mm)with a
negative photoresist EPON SU-8 bought from Microlithography Chemical corp.
The process is basically the same as described by M. Despont et.al. in
their paper "High-aspect-ratio, ultrathick, negative-tone near-UV
photoresist for MEMS applications". But the EPON patterns I made have very
sharp edges, as I can see from the vertical profile of the
structures, the EPON surface layer extends out in a sharp angle like
a bird's beak. I wonder if anyone experienced the same problem and knows
how to get rid of the problem. Any comments/suggestions from you will be
highly appreciated.

- Hui

 ~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
Hui Tang

Research Assistant
BioMEMS Labratory, Beckman Institute
ECE Dept., Univ. of Illinois at Urbana-Champaign
Tel: (217) 265-0827(Lab), 333-0188(O), 356-7637(H)
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
Addison Engineering
University Wafer