MEMSnet Home: MEMS-Talk: Ni and Cr etching
Ni and Cr etching
2006-01-31
biqin huang
2006-01-31
Brent Garber
2006-01-31
Neal Ricks
Ni and Cr etching
Brent Garber
2006-01-31
Bq,

Cr-7 etch for Cr and either a commercial Ni etch or mix 10% HNO3 / H2O.

Brent

biqin huang wrote:

> Does anyone kow the etchants for Ni and Cr which doesn't attack Gold thin
> film?