Photoresist RIE
2006-02-08
K. V. Sridhar
2006-02-08
Michael Prömpers
2006-02-08
Hongjun-ECE
2006-02-17
Yanjun (David) Tang
2006-02-09
David Kallweit
Photoresist RIE
K. V. Sridhar
2006-02-08
Hello All,

I am using photoresist AZ5214 (thickness 1.5um) as a
mask for my ICP-RIE process(SF6 gas ) and the resist
dosent last for more than 2 min . I am  looking for a
photoresist that would last atleast 10 min. Can anyone
suggest a process involving photoresist lasting for
more time regarding the above.

Thanks
Sridhar

Kuchibhatla Venkata Sridhar
MSEE, West virginia University, Morgantown ,
WV 26505, USA
304-685-8523(M)
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
University Wafer
Addison Engineering
Mentor Graphics Corporation