MEMSnet Home: MEMS-Talk: decrease total thickness variation
diffusion barrier for copper-polyimide
2006-02-10
erkin seker
2006-02-10
Michael D Martin
PVDF vendor
2006-02-10
Shivalik Bakshi
decrease total thickness variation
2006-02-11
Andrea Mazzolari
2006-02-12
shay kaplan
2006-02-13
gtomblin
2006-02-17
Bill Moffat
decrease total thickness variation
shay kaplan
2006-02-12
Andrea
Ask you vendor for a low TTV wafer. They are the ones equipped to do this.
shay

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Andrea Mazzolari
Sent: Saturday, February 11, 2006 1:10 PM
To: General MEMS discussion
Subject: [mems-talk] decrease total thickness variation

Is there a way to decrease or eliminate total thickness variation in a
silicon wafer ?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Mentor Graphics Corporation