MEMSnet Home: MEMS-Talk: Electroplating Equipment Set-up
Electroplating Equipment Set-up
2006-03-05
J.J wang
2006-03-05
g.balsubra manian
2006-03-20
J.J wang
2006-03-20
g.balsubra manian
AZ4562
2006-03-21
steph champ
2006-03-21
Shay Kaplan
2006-03-21
abdou sar
2006-03-22
steph champ
Electroplating Equipment Set-up
J.J wang
2006-03-05
Hi, Everyone

I am trying to do electroplating copper for about 2 to 5 um thickness on top of
the sacrificial layer of polymer.

Right now my lab has EPI E-Brite Ultra Cu solution, multimeter, hotplate,
magnetic stiring bar,voltage source, electrode clamps. I connected the circuits
with required current (10ASF), but seems the copper didn't grow on the seed
layer which is also copper.

I went back to the instruction sheet of the E-Brite Ultra Cu, it looked much
more complicated than I thought. Does anybody have the experience using the
E-Brite Ultra Cu solution ? Please give me some brief description of how to us
it.

My another question is: Can I use other materials as seed layer such as
aluminium ?

Any help will be appreciated. If you have experience with other plating
solutions, it is also welcome, I don't have to restrain to one only material.

Thanks
J.J.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
University Wafer
Process Variations in Microsystems Manufacturing