Re: Information on Thick Film Hybrid Technologies
1998-03-02
Paul W. Green
Re: Information on Thick Film Hybrid Technologies
Paul W. Green
1998-03-02
At 10:57 AM 2/25/98 , you wrote:
>To whom it may concern,
>
>I am starting off in the domain of thick-film hybrid technologies, and
would like to know more about the field.
>
>First of all, do any good general reviews exist on the subject? I am
particularily interested in the piezoresistive effects, piezocapacitive
effects, photoacoustic effects, etc.
>
>Secondly, what products utilise this technology? I have already heard of
pressure and vibration sensor products, thickfilm circuits for LAN
applications such as routers, communication products such as cellular
telephones & GPSs.

RAFAL...

Can you copy me in on the replies you receive...

thanks

>
>Thank you,
>
>Rafal
>
>~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
~~~
>  Dr. Rafal Romanowicz
>  Institut de Production en Microtechnique
>  IPM-EPFL
>  CH-1015 Lausanne, Switzerland
>  Phone:  (+41) 21 693 58 60
>  Fax:    (+41) 21 693 58 59
>  e-mail: [email protected]
>  URL:    http://dmtwww.epfl.ch/imt/gp
>~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
~~~
>
>
>
>


Regards

Paul W. Green



|||||||||||||||||||||||||||||||||||||
Nanothinc
433 Town Center-701
Marin County, Ca.94925  USA

Web Site:      http://www.nanothinc.com

Voice Mail:    1 415 680 1596
EMail:           [email protected]
                    [email protected]
Tel:               1 415 927 9557
Fax:              1 415 680 1596
||||||||||||||||||||||||||||||||||||||


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing
University Wafer