MEMSnet Home: MEMS-Talk: sputtering of metal on wet etched glass substrate
sputtering of metal on wet etched glass substrate
2006-04-13
Rupesh Sawant
DRIE Process Enquiries
2006-04-19
K A Chan
2006-04-19
Jim Beall
2006-04-20
Pradeep Dixit
2006-04-20
Julie Verstraeten
2006-04-13
Jauniskis, Linas
sputtering of metal on wet etched glass substrate
Rupesh Sawant
2006-04-13
Is sputtering possible on a wet etched glass substrate. Especially
when electtrode has to be sputtered in the wet etched microchannel. i
have a reference in which the sputtering can be done on an etched
glass channel. But in that case the depth of the glass microchannel is
8 um. So the sides of the microchannel is almost vertical.  The depth
of my microchannels on glass is 50 um. So in my case the isotropic
etching will have lot of effect on the side walls of the channel. Can
sputtering assure me a continuos electrode length within the channel.

--
RUPESH SAWANT
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
MEMStaff Inc.
MEMS Technology Review