MEMSnet Home: MEMS-Talk: PDMS bonding.,
PDMS bonding.,
2006-06-10
g.balsubra manian
2006-06-12
Joseph Grogan
2006-06-13
Gareth Jenkins
2006-06-13
Joseph Grogan
2006-06-14
Gareth Jenkins
2006-06-14
Joseph Grogan
2006-06-13
Ali Bhagat
2006-06-15
Gareth Jenkins
2006-06-13
lumiaoÂÀÃç
2006-06-15
huy vo
PDMS bonding.,
g.balsubra manian
2006-06-10
Guys.,

What is the bonding time for oxidised PDMS with the
oxidised glass.

Whether bonding occurs immediately after the surfaces
get into contact.

Thanks

Bala.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMStaff Inc.
Addison Engineering
The Branford Group