MEMSnet Home: MEMS-Talk: Pt etchant
Pt etchant
2006-06-22
Jeehwan Kim
2006-06-22
Kirt Williams
2006-06-22
Michael D Martin
Pt etchant
Kirt Williams
2006-06-22
Use warm or hot aqua regia. It won't etch Si or SiO2, but does etch Pt.
Check for papers online regarding etch rates for micromachining...
    --Kirt Williams

----- Original Message -----
From: "Jeehwan Kim" 
To: 
Sent: Thursday, June 22, 2006 1:51 PM
Subject: [mems-talk] Pt etchant


> Dear colleagues,
>
> I will use the Pt to protect my Si wafer surface for anodization. Is there
> any one who has a recipe for removing Pt without attacking Si surface?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
Process Variations in Microsystems Manufacturing
MEMStaff Inc.