DRIE - Heating Effects & influence on CMOS
Micro Sense
2006-06-28
>
> Mike and Martin, thanks for your inputs. Martin, yes I also experienced
> the same problems you'd mentioned. Passivating a bit longer should help in
> minimizing over-etching/notching.


- VJ