2006-07-20
RABBIA Laurent
2006-07-20
shay kaplan
Re: RE: [mems-talk] Spin coating for silicone material
2006-07-21
Kevin Christ
2006-07-20
pradeep # sharma
2006-07-20
Shile
Spin coating for silicone material
pradeep # sharma
2006-07-20
Dear Laurent,
Please refer to Nature Publishing group. A couple of months ago there was a
paper by a Japanese group to spin coat Si using solution and then devloping that
to get Si thin film of about 50 to 200 nm. They also made thin film transistor
out of Si thin film.

Good Luck...Pradeep Sharma.


On Thu, 20 Jul 2006 RABBIA Laurent wrote :
>Hello everybody,
>
>I would like to deposit silicone by spin coating in order to control the
>thickness of the layer. Has someone already done that ?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
The Branford Group
Mentor Graphics Corporation