Burned Photoresist
2006-07-20
Martin Aguilar
2006-07-20
Ad Hall
2006-07-20
[email protected]
Burned Photoresist
[email protected]
2006-07-20
If only aluminum is exposed on the wafer after ion milling I would suggest
using a fluorine etch CF4+ O2 to remove the fences in your rie system. The
fluorine won't attack the Al much and it should remove the Carbon left behind
from your milling process. You might also try doing a photoresist stabilizing
with UV and temperature to harden the resist prior to ion milling. This might
provide some protection. Bob Henderson
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Tanner EDA by Mentor Graphics
Addison Engineering