pradeep # sharma
Electroless Plating of Ag on Silicon?
pradeep # sharma
2006-07-31
Dear All,
Please suggest me exact method to do electroless plating of Ag on Si. I wish to
know details like concentration of different chemicals used, temperature of the
Ag plating bath and pH etc.

A internet link of related papers/journals and information is welcome.

Thanks a lot.

with regards,
Pradeep Sharma.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
MEMStaff Inc.
Process Variations in Microsystems Manufacturing