MEMSnet Home: MEMS-Talk: Honeywell SOG 512B Etching Recipe with LPCVD SiliconNitride Selectivity (Abdel Moneim Marzouk)
Honeywell SOG 512B Etching Recipe with LPCVD Silicon Nitride Selectivity (Abdel Moneim Marzouk)
2006-08-02
Abdel Moneim Marzouk
Honeywell SOG 512B Etching Recipe with LPCVD SiliconNitride Selectivity (Abdel Moneim Marzouk)
2006-08-02
Ad Hall
Honeywell SOG 512B Etching Recipe with LPCVD SiliconNitride Selectivity (Abdel Moneim Marzouk)
2006-08-03
Shay Kaplan
Honeywell SOG 512B Etching Recipe with LPCVD SiliconNitride Selectivity (Abdel Moneim Marzouk)
Shay Kaplan
2006-08-03
Abdel Moneim
Try using SF6

Shay Kaplan
Tel:972-4-6442492
Fax: 972-4-56442803
Mob: 972-54-7453102.
Mail: [email protected]
Visit us: www.mizur.com

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Abdel Moneim Marzouk
Sent: Wednesday, August 02, 2006 5:05 PM
To: [email protected]
Subject: [mems-talk] Honeywell SOG 512B Etching Recipe with LPCVD
SiliconNitride Selectivity (Abdel Moneim Marzouk)

Hi,

I am currently working on developing a process that involves Honeywell's
Spin-on-Glass (SOG) 512B that is deposited on LPCVD Silicon Nitride wafers.
I am using a RIE dry etch to pattern the SOG, and apparently my recipe
etches the nitride faster than it does the SOG. The recipe I am using
includes CHF3 (40 sccm flow rate), Ar (70 sccm), and CF4 (7sccm).

This recipe etches SOG at a rate of 0.20 microns/min, and nitride at
0.5 microns/min. Since my main concern is etching SOG, and I need the
nitride for insulation puroposes, I was looking for an alternative RIE etch
that would be selective to LPCVD silicon nitride.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review