Jeehwan Kim
2006-08-03
Oliver Horn
2006-08-03
Jeehwan Kim
2006-08-03
Michael D Martin
2006-08-04
Oliver Horn
Pt on Si
Michael D Martin
2006-08-03
Jeehwan,
   HF etches Ti.

-Michael Martin


>>> "Jeehwan Kim"  08/03/06 4:26 PM >>>
Hi Oliver,

I deposite 200nm Pt on Si with 50A Ti adhesion layer via e-beam
evaporator
and then put that into HF solution. Pt was removed (peeled off) after
several minute. Is that difference coming from machine we used?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
MEMStaff Inc.
Addison Engineering