K. Winglee
thermal evaporation of nickel
K. Winglee
2006-08-07
Hi,
  I am trying to deposit nickel using a thermal evaporator. I am using nickel
powder. However, the nickel does not always evaporate off the boat. Does anyone
have any suggestions on how to get the nickel to deposit?
  Thanks,
  Kathryn Winglee
  Undergraduate
  University of Washington