MEMSnet Home: MEMS-Talk: Release agent(PDMS-Silicon)
Release agent(PDMS-Silicon)
2006-08-15
Z xy
2006-08-15
g.balsubra manian
2006-08-15
Jim Beall
2006-08-15
Hunter, Luke L
Release agent(PDMS-Silicon)
g.balsubra manian
2006-08-15
You can use acetone . I am using acetone to simply
release the mold.

Bala.


--- Z xy  wrote:

> Hi,
> We are looking for a type of mold release agent used
> for stripping off the
> PDMS layer from the silicon mold in nanoimprint fab.
> We basically want to
> make it much easier to strip off the thermal cured
> PDMS layer from the
> nanopatterned silicon template. Can anyone tell us
> where to buy such
> release agent or if there is any other solutions?
> Rayne
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation