MEMSnet Home: MEMS-Talk: indium deposition/plating
indium deposition/plating
2006-08-24
Vinay
2006-08-25
Kirt Williams
indium deposition/plating
Kirt Williams
2006-08-25
A related and possibly easier method is buy indium foil, lay it between the
surfaces, and heat slightly.
The Indium Corporation of America sells indium and many alloys with
different melting points in foil format.
    --Kirt Williams

----- Original Message -----
From: "Vinay" 
To: 
Sent: Thursday, August 24, 2006 11:34 AM
Subject: [mems-talk] indium deposition/plating


> Hello,
> I am looking for companies which have the capability of depositing
> induim on a gold surface. We wish to stick together 2 gold surfaces
> and want to use indium as a sealing agent.
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
Addison Engineering
Mentor Graphics Corporation