A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Plasma chamber
Plasma chamber
2006-08-29
amron gary
2006-08-29
Scott McWilliams
2006-08-29
David Henriks
2006-08-29
Bill Moffat
Evaporation of Silica
2006-08-30
Sreemanth M Uppuluri
2006-08-30
shay kaplan
hardbaked photoresist...
2006-08-30
Jan Michael Kubr
2006-08-30
Jack Mulligan
2006-08-30
Bill Flounders
2006-08-31
[email protected]
Plasma chamber
amron gary
2006-08-29
Hello all,

I want build a chamber for Fluorine gas plasma. My
questions are:

1. Does someone has plasma chamber for Fluorine gas?
2. Can someone on this forum help me in building this
chamber?
3. What gases can be used to create the plasma of
flurorine? C2F2 or C2F4 or C2F6??? Thanks in advance..

Gary amron
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Harrick Plasma, Inc.
Mentor Graphics Corporation