MEMSnet Home: MEMS-Talk: Cutting chips with fragile free-standing devices into small pieces
Cutting chips with fragile free-standing devices into small pieces
2006-09-04
D. Zhou
Cutting chips with fragile free-standing devices into small pieces
2006-09-05
Nicolas Duarte
2006-09-05
Torsten Wagner
Cutting chips with fragile free-standing devices intosmall pieces
2006-09-05
gilgunn
Cutting chips with fragile free-standing devices intosmall pieces
2006-09-06
Kagan Topalli
Cutting chips with fragile free-standing devices into small pieces
Nicolas Duarte
2006-09-05
The best possible solution would be to release it after you have done
the dicing.

Another option which only sometimes works is to coat the finished
device in photoresist before dicing.  As long as your device does not
succumb to stiction from the PR or the solvent you later use to
remove the PR you should be ok.

Nicolas Duarte
PhD Student
Penn State University
Electrical Engineering

At 3:39 PM +0100 9/4/06, D. Zhou wrote:
>Dear all,
>
>I am fabricating some free-standing MEMs devices based on SOI wafer.
>Now I need to cut the chips into individul devices to do some
>measurements. The problem is that the structure is so fragile that
>when cutting it using scriber and breaking it with hands the whole
>structure collapses. Could anyone who has been faced with the same
>problem please give me any suggestions?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
The Branford Group
Nano-Master, Inc.