Adhesive layer for gold on oxide and patterning
2006-09-08
J.J HU
2006-09-08
walter essinger
2006-09-12
Kirt Williams
Adhesive layer for gold on oxide and patterning
J.J HU
2006-09-08
Hi all,
I am trying to put down 300~500nm Au film on Si dioxide as electrodes, and I
am just wondering what kind of adhesive layer (needs to be electrically
conductive) should I deposit before Au to improve the adhesion?

And anyone has some good thoughts about how to pattern the gold electrode
(as well as the adhensive layer)? Will regular lift-off work?

Thanks much,
JJ Hu


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing