MEMSnet Home: MEMS-Talk: To remove Al layer from PMMA/glass substrate
To remove Al layer from PMMA/glass substrate
2006-10-13
Hyunsoo Park
2006-10-13
Mathieu Foquet
2006-10-16
Hyunsoo Park
2006-10-16
Mathieu Foquet
To remove Al layer from PMMA/glass substrate
Hyunsoo Park
2006-10-16
Thank you for reply.

I can't use gold right now. could anyone tell the solution to remove
Al layer without any damage to PMMA?

Otherwise, could anyone tell me another way to use glass substrate in
E-beam lithography?

Thank you.


On 10/13/06, Mathieu Foquet  wrote:
> Any reason you're not using 5 to 10nm gold and then use a mix of KI/I2
> gold etch. I have asimilar ebeam process and this recipe has worked well
> for me.
>
> To my knowledge, Aluminium is more delicate to remove without moving to
> aggressive chemistries that would also affect your pmma.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Addison Engineering
MEMStaff Inc.