MEMSnet Home: MEMS-Talk: Wet etching SiN with photoresist
Wet etching SiN with photoresist
2006-10-28
蘇俊榮 Chun-Jung Su
2006-10-31
Scott McWilliams
2006-10-31
R Zhang, Electrical & Electronic Engineering
2006-10-31
Avi Laker
Wet etching SiN with photoresist
Scott McWilliams
2006-10-31
Hi CJ, I think most people use phosphoric acid for SiN etching, BOE works
well for PECVD SiN but not thermal nitride.

Regards,

Scott
----- Original Message -----
From: "??? Chun-Jung Su" 
To: 
Sent: Saturday, October 28, 2006 12:53 PM
Subject: [mems-talk] Wet etching SiN with photoresist


> Dear all,
>
> I am trying to etch 1000A-thick SiN with photoresist. I have used B.O.E.
> to
> etch the SiN formed by our LPCVD system, but the etching rate is quite
> low,
> i.e. 12 A/ min. Is there any other chemical solution to accomplish this
> job?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
MEMS Technology Review
Tanner EDA by Mentor Graphics