Nickel electroless Plating!!
Seth Burtner
2006-11-03
Hello Madhav,

You can purchase an electroless nickel plating kit, a company called
Transene used to sell this but, I am not sure if they still do.  The
kits are relatively inexpensive.
The adhesion to PMMA may present an issue however I am not sure of this.
If you would like to contact me directly please feel free to do so.

Best Regards,

Seth Burtner

[email protected]
-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of madhav rao
Sent: Thursday, November 02, 2006 7:48 PM
To: General MEMS discussion
Subject: [mems-talk] Nickel electroless Plating!!

Hi All,
        I am not able to find a simple way of doing
electroless Nickel plating on PMMA patterned silicon
wafer. Can any one provide me any PDF file or any
procedure to do Electroless Nickel plating.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Harrick Plasma, Inc.
Mentor Graphics Corporation