MEMSnet Home: MEMS-Talk: how to mask AL pattern while doing Bulkmicomachining
how to mask AL pattern while doing Bulkmicomachining
2006-11-06
abhaya joshi
how to mask AL pattern while doing Bulkmicomachining
abhaya joshi
2006-11-06
dear friends,
i am having patterned AL layer on si wafer. In my case, I have to etch si
for 180 micron, but as Al layers is there, i am unable to mask it with Sio2
or Si3n4.
i am using 30wt % KOH at 70-80C as Si etchat.
So please suggest me propable solution in this case.
with regard
abhay joshi,
university of pune
india
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Harrick Plasma, Inc.
Addison Engineering