Silicon Designs, Inc. is near Seattle.  We have the capabilities to do
what you ask.  Are you talking about etching into the Aluminum 25
microns?   It would depend on exactly what you were after whether or not
we could do it.

 --Jason Tauscher
 Silicon Designs, Inc.
 [email protected]

 -----Original Message-----
From: Jim Intrater -- FR [mailto:[email protected]]
Sent: Tuesday, June 09, 1998 5:25 PM
To: [email protected]
Subject: 


I need to find a company (preferably, but not necessarily, on the west
coast) that can apply a resist layer to a 2.5" square of aluminum oxide
and image some 1 mil (25 microns) wide, free-standing bars at at least 1
to 2 mils (25 to 50 microns) tall. Do you have any suggestions?




 Jim Intrater
 Oryx Technology Corp.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
MEMS Technology Review
Nano-Master, Inc.