WG: Silicone spin coating of steel membranes
2007-07-03
Markus Herz
2007-07-03
Bill Moffat
WG: Silicone spin coating of steel membranes
Markus Herz
2007-07-03
Hello community,

In a prior project we spin coated steel membranes with silicone, but
adhesion was not satisfying. Metal is not a good adhesion partner for
silicone, roughening or a primer would perhaps help. Any other
recommendations are greatly appreciated!


Best regards

Markus Herz



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Addison Engineering
Harrick Plasma, Inc.