MEMSnet Home: MEMS-Talk: Re : SiC and quartz materials
Re : SiC and quartz materials
1998-07-27
Christophe Sudre
Re : SiC and quartz materials
Christophe Sudre
1998-07-27
This is a multi-part message in MIME format.
--------------1CC7ED4CC4746F718F8BFAC0
Content-Type: text/plain; charset=us-ascii
Content-Transfer-Encoding: 7bit

Hi

What follows is a good summarry of the SiC stuff. I hope it will help
you.

Christophe


http://www.csc.fi/sic/contents.html

--
 _______________________________________________________________________________
| Dr Christophe Sudre                             Fax :   353 21 270271
|
| Research Scientist                              Phone : 353 21 904079
|
| University College Cork                         WWW :
http://www.nmrc.ucc.ie/|
| National Microelectronics Research Center       Email: [email protected]
|
| Lee Maltings, Prospect Row
|
| Cork, Ireland
|
|_______________________________________________________________________________
|



--------------1CC7ED4CC4746F718F8BFAC0
Content-Type: text/html; charset=iso-8859-1; name="contents.html"
Content-Transfer-Encoding: 8bit
Content-Disposition: inline; filename="contents.html"
Content-Base: "http://www.csc.fi/sic/contents.html"


 
SiC page





SiC Research

  • SiCEPS, Silicon Carbide Electrical Powder Systems, a national research project in Sweden.
  • SiC electronics group at Industrial Microelectronics Center, Stockholm. Mostly power devices. A motivation for SiC research.
  • Linköping University, Growth and charcaterisation for optoelectronic and power device applications, Mikael Syväjärvis page on SiC growth.
  • PhysTech-WBG, Physics & Technology of Wide BandGap Semiconductors. Based at the Ioffe Institute in St.Petersburg.
  • SiC page by Wirgil Shields, The Jet Propulsion Laboratory's SiC technology development program.
  • SiC electronics at NASA Lewis Research Center, Cleveland, Ohio. Examples of SiC-based electronics in hostile environments, Recent developments.
  • Purdue WBG, Wide band gap semiconductor device research program at Purdue University.
  • SiC Research at Auburn University, mostly device technology
  • SiC Research at Case Western Reserve University. Also first-principles computations of SiC properties.
  • Nanolab, wide-bandgap semiconductor research, particularly thin films of SiC, at University of Cincinnati's Nanoelectronics Lab.
  • CSC, modeling of silicon carbide crystal growth phenomena.

SiC Business

  • Cree Research Inc., provider of SiC wafers and LEDs. Dominating player in the field.
  • Epitronics, wide bandgap materials, including SiC wafers.
  • SiCrystal AG, development and manufacturing of SiC wafers.
  • TDI, Technologies and Devices International, Inc., SiC wafers.
  • Morton's SiC, commercial CVD grown layers of SiC.
  • Sterling Semiconductor, manufacturer of silicon carbide materials for semiconductors.
  • Novecon Technologies, single-crystal SiC. Particularly SiC related patents, US and Internatinal.
  • Wafer Technology, particularly SiC wafers.
  • Boston Electronics Corporation, electronic and optical materials and devices, particularly SiC photodiodes.
  • Blue SiC LEDs by Siemens
  • Hoya Corporation, 3C-SiC on Si substrate.
  • Northrop Grumman Corporation High power microwave, temperature-tolerant, and radiation-hard electronics based on WBG semiconductors, SiC and GaN
  • EMCORE, EMCORE Corporation manufactures deposition systems for the production of advanced semiconductor materials.
  • Aixtron, company for CVD engineering.
  • Epigress AB, Process equipment for bulk and CVD growth of SiC.
  • 3C Semiconductor Corporation Technolgy for SiC semiconductor devices.

SiC Information

  • HITEN High Temperature Electronics Network. Lot of information and links.
  • Silicon carbide page, including links and introduction to SiC. Emphasis on ceramic SiC.
  • Many of the articles on SiC are published in The Journal of The Electrochemical Society and Journal of Crystal Growth.
  • Picture of the SiC crystal structure at CalTech
  • AFM image of SiC screw dislocation of SiC by Park Scientific Instruments.
  • SiC [110], a high resolution image at University of Melbourne.

SiC Happenings

  • ICSCIII-N '97, International Conference on Silicon Carbide, III-Nitrides and Related Materials - 1997, was held in Stockholm August 31 - September 5 (Proceedings). Next conference will be organized by Cree Research Inc. It will be held in Durham, North Carolina in autumn 1999.
  • ICCG 12, The Twelfth International Conference on Crystal Growth, Jerusalem, Israel, July 26-31, 1998.
  • ECSCRM'98, 2nd European Conference on Silicon Carbide and Related Materials, Montpellier, France, September 2-4, 1998.

Crystal Growth Modeling

  • CVD Sciences at Sandia Laboratories, Simulations: general CVD, massively parallel, Design optimization.
  • CVD Research at Colorado State University, particularly Chemkin manuals and recent publications, Software tools for reactive gases.
  • TCC, a CHEMKIN based interactive WWW tool which carries out calculations for reacting ideal gas mixtures (e.g. the Si-C-H system).
  • Process Modeling on WWW Virtual Library.
  • CFD Resources Online A very comprehensive list of CFD related services maintained by Jonas Larsson.
--------------1CC7ED4CC4746F718F8BFAC0--
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Addison Engineering
MEMS Technology Review
Process Variations in Microsystems Manufacturing