Hi guys,

I am trying to etch back a Si bulk with KOH to remain a ~10 um thick membrace
wirh an area of 0.5mm x 0.5mm. I am concerned if such a thin membrance with such
a big area is very fragile and if it is achievable. Someone told me such a thin
Si layer is not flexible as a thin nitride layer. Is that true? I appreciate
your advices.

Lawrence
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Mentor Graphics Corporation