Hi all,
i need to realize holes of size 20x15mm in (110) silicon wafers. 20mm size
is aligned with (111) planes. Alignement with (111) planes is not crucial.
After LPCVD silicon nitride deposition and patterning i'm planning to use
KOH etch to realize the holes. I know that K ions will diffuse in the
silicon. Will this alter crystalline quality of the surfaces exposed to
KOH etch inducing some types of defects ?

Many thanks,
Andrea

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
MEMS Technology Review
Process Variations in Microsystems Manufacturing