Anneal recipe for Pt thin film on Si wafer
2008-02-28
Miyakawa, Natsuki
2008-03-03
Oliver Horn
2008-03-05
Michael D Martin
2008-03-05
Gary Hillman
2008-03-05
Miyakawa, Natsuki
Anneal recipe for Pt thin film on Si wafer
Michael D Martin
2008-03-05
I've had this problem in the past, i.e. formation of Pt-Si alloys during an
anneal with (I think) a Cr adhesion layer.  Could anyone recommend a material
stack Pt/ adhesion layer/ diffusion barrier?

Thanks,
   Michael
   U. of Louisville

>>> Oliver Horn  3/3/2008 4:38 AM >>>
Hello Natsuki,

you will get PtSi or PtSi2 if you heat up Pt on Si without diffusion
barrier, even at 260°C.  The adhesion is only a bit improved.

Oliver
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
University Wafer
Addison Engineering