Xinyu Li
2008-03-10
Hello friends in MEMS and microfluidics,

If I want to use a solution flow through microchannel to treat PDMS
surface by using trichlorosilane, anybody has some standard procedure
for this type of work?

Thanks.

XL

Xinyu Li, PhD
RainDance Technologies