2008-05-20
Satish Yeldandi
2008-05-20
Andrew Sarangan
2008-05-20
Satish Yeldandi
2008-05-20
Ngo Ha Duong
2008-05-20
Tolga YELBOGA
2008-05-20
Oakes Garrett
2008-05-21
Jason Milne
2008-05-23
Jie Zou
2008-05-23
乔大勇
PR removal after ICP RIE etching
Satish Yeldandi
2008-05-20
Thanks for the reply.I am using AZ 5214E and AZ P4400 photo resists.

On Tue, May 20, 2008 at 10:05 AM, Andrew Sarangan  wrote:
> What type of photoresist?
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMStaff Inc.