MEMSnet Home: MEMS-Talk: KMPR on Ag layer
KMPR on Ag layer
2008-05-26
Mei Liu
KMPR on Ag layer
Mei Liu
2008-05-26
Hi,

I am using photoresist KMPR on silver layer, for later DRIE. But the photoresist
seems very subtle.Does anyone know the exact exposure energy of this
photoresist?And when I etched silver after PR, undercut happened badly. Even
after DRIE, when removing KMPR residue by Remover RG, silver will peel off too.
Is this because the adhesion between silver and silicon is very weak? If yes,
how can i enforce the adhesion?

Thanks.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Nano-Master, Inc.