MEMSnet Home: MEMS-Talk: metal on tungsten (Andrea Mazzolari)
metal on tungsten (Andrea Mazzolari)
2008-05-26
saravan kallempudi
metal on tungsten (Andrea Mazzolari)
saravan kallempudi
2008-05-26
 Hi,

If you want deposit 20 micron only best suitable way is electroplating. But its
not advisable to go for electroplating with gold/platinum in terms of cost.
Normally Cu/Ni cane deposited easily with above method. If you are more specific
why you are using W may be senior members of the group can help you.


Kallempudi Sreenivasa Saravan

PhD student, Electronics Engineering,
1054, FENS, Sabanci University,
Orhanli, 34956,
Tuzla, Istanbul, Turkey.


-Hi all,

i need to deposit about 20um of any metal on tungsten.
Could someone suggest a metal which have good adhesion to tungsten and an
appropriate deposition technique ?

For my understanding Titanium deposited by electrodeposition should work
fine, but i don't have a big experience.

Many thanks,
Andrea
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review