Hi:

  I plan to do spin coating on a silicon wafer.  Polyimide UR3 100 and
UR3 140 are discribed in the papers I read.  But I can not find them.
Does anyone know where I can find them?

  Thanks for help.






==
------------------------------
Gang Sun
Department of Physics
Wayne State University
666 W. Hancock St.
Detroit, MI 48201
email: [email protected]
_________________________________________________________
DO YOU YAHOO!?
Get your free @yahoo.com address at http://mail.yahoo.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
University Wafer
Mentor Graphics Corporation
The Branford Group