MEMSnet Home: MEMS-Talk: Under what conditions is buffered-HF (BOE) etching diffusion limited?
Under what conditions is buffered-HF (BOE) etching diffusion limited?
2008-09-15
Ken Healy
2008-09-15
Shay Kaplan
2008-09-15
Koray Karakaya
2008-09-16
Ken Healy
Under what conditions is buffered-HF (BOE) etching diffusion limited?
Shay Kaplan
2008-09-15
Are you using BOE with surfactant?

Shay

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Ken Healy
Sent: Monday, September 15, 2008 6:22 AM
To: [email protected]
Subject: [mems-talk] Under what conditions is buffered-HF (BOE)
etchingdiffusion limited?

Hello,

Is anyone aware of the conditions under which buffered-HF (BOE) etching is
diffusion limited, or a reference which discusses this?

The particular situation I'm interested in is etching a 5um thick silicon
dioxide layer at the bottom of a KOH-etched pit in silicon, as shown below.
The silicon is 500um thick and base of the pit (top in the
diagram) is ~ 100um x 100um.


membrane nitride
======================================================================
dielectric oxide               |        |
--------------------------------        ------------------------------
                               /          \
                              /            \
silicon                     /              \
                            /                \
                           /                  \
--------------------------                    ------------------------
mask oxide               |                    |
==========================                    ========================
mask nitride


I have measured the etching rate of my 6:1 BOE solution to be 60nm/min on
fully exposed oxide. I suspect the etching rate in this case may be
diffusion limited due to the geometry, because, after 2h20min the oxide
still does not appear to be fully etched. My doubt is due to the fact that
it is hard to measure the the actual thickness in this case. All I have to
go on are SEM images showing undercut, which suggests at least some etching,
and TEM observations where the electron beam is scattered so much it is
impossible to focus the beam at high magnifications.

Regards,

Ken Healy

Dept of Physics and Astronomy
University of Pennsylvania

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Tanner EDA by Mentor Graphics
MEMStaff Inc.