A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: how to test porosity of deposited layer ?
how to test porosity of deposited layer ?
2008-09-20
[email protected]
2008-09-20
Brad Cantos
2008-09-21
Bill Moffat
how to test porosity of deposited layer ?
[email protected]
2008-09-20
hi

i have deposited SiO2 by PECVD. Now i want to test the quality of the film
more specifically i want to check the porosity of the deposited film
please tell me how i can test porosity.

--
Kamlesh Pawar
M.Tech (Biomedical Engg)
Mob :+919870062960
IIT-Bombay

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
Addison Engineering
Process Variations in Microsystems Manufacturing