A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Re: Spin coating of the THICK PMMA
Re: Spin coating of the THICK PMMA
1998-09-13
Jayant Neogi
1998-09-14
Armin Kuebelbeck
1998-09-30
Skrobis, Ken
Re: Spin coating of the THICK PMMA
Armin Kuebelbeck
1998-09-14
For the coating I don't have a proper solution, but for the adhesion you
should try to use an adhesion promoter. Union Carbide has some excellent
types with functional groups. They call it SILAN.

Armin Kuebelbeck

______________________________________________________
Get Your Private, Free Email at http://www.hotmail.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing