A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Spacer material
Spacer material
2008-11-12
Nicolas Vergauwe
2008-11-12
Morten Aarøe
2008-11-12
Brad Cantos
2008-11-12
SEBESTA Edward
2008-11-12
Shay Kaplan
2008-11-12
Gareth Jenkins
2008-11-12
Krueger, Bernd
2008-11-12
[email protected]
Spacer material
SEBESTA Edward
2008-11-12
Just a thought.

If I remember correctly, very thin foils are provided on backing materials. They
are very uniformly coated with an adhesive. In contact to another substrate they
adhere with the adhesive. You then peel off the backing. I think I remember
seeing them used in art projects. You just need one that is silver without a
coating. For prototyping it might work.

Ed


-----Original Message-----
From: [email protected] [mailto:[email protected]] On
Behalf Of Nicolas Vergauwe
Sent: Wednesday, November 12, 2008 2:43 AM
To: [email protected]
Subject: [mems-talk] Spacer material

Hi everyone,

Could you suggest me a spacer material for separating two (horizontal) glass
plates? The spacer should have a thickness of 100 µm, but more importantly, the
thickness tolerance should be as low as possible. Also, the spacer needs to be
fixed manually on the glass plate: it cannot be processed on the glass plate but
it has to be attached afterwards.

I thought of using a thin metal sheet and then glue it to the glass plate, but I
don't know if it will be the best way.

Any help or ideas are welcome!

Nicolas
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Nano-Master, Inc.
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics