MEMSnet Home: MEMS-Talk: Stress reduction in SOI
Stress reduction in SOI
2008-12-15
Jason Milne
2008-12-15
Andrea Mazzolari
2008-12-16
Jason Milne
2008-12-15
Michael
2008-12-16
[email protected]
2008-12-19
Trent Huang
Stress reduction in SOI
Andrea Mazzolari
2008-12-15
Hi Jason,

> I purchased some thin SOI recently to make some fixed-fixed beams and
> cantilevers, and I was assuming that the device layer would be close to
> zero stress (slightly tensile, if anything) and have no stress
> gradients. Having made the structures, it seems that the device layer is
> compressively stressed (the fixed-fixed beams buckle) and has a stress
> gradient (the cantilevers curl upwards). I was wondering if anyone has
> tried to anneal SOI wafers to reduce stress and/or stress gradients, and
> if so, what conditions did you use?

Which kind of SOI are you using ?
For my experience if you use SIMOX SOI you should not have this kind of
problem.

Andrea

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Nano-Master, Inc.
MEMStaff Inc.