2009-01-29
basar bolukbas
2009-01-29
Bill Moffat
2009-01-30
basar bolukbas
2009-01-30
Bill Moffat
2009-01-30
basar bolukbas
2009-01-30
Edward Sebesta
2009-01-30
basar bolukbas
2009-02-02
Edward Sebesta
Double lithography problem with SU1828-TI35ES
basar bolukbas
2009-01-30
Hello Bill,

First of all, please forgive me beacuse i am a rookie for this kind of
''advanced process''.
And, i am appriciate for your great helpings. But i unfortunately, i have still
questions to you.
Do you suggest that i should coat HMDS on top of first resist before second
lithography?
After HMDS what should i do? Do i have to make O2 plasma or just HMDS spin
coating is enough for me in order to make another lithography?

Again thank you for your help.

Best Regards.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMS Technology Review
Nano-Master, Inc.
Harrick Plasma, Inc.