Re: Deposition at below zero
1998-09-22
Paul McGrath
1998-09-22
Carlos Mastrangelo
1998-09-22
Carlos Mastrangelo
1998-10-10
Greg White
Re: Deposition at below zero
Carlos Mastrangelo
1998-09-22
You can deposit films by UV photopolymerization at very low
temperatures --reported down to -10C back in the mid 70s.

                                        -CHM

On Wed, 9 Sep 1998, lee ki seong wrote:

>
> hello, colleague
> It might be silly question to somebody.
>
> but I think it's impossible.
>
> Is there anybody who try to deposit some film at very low temperature.
>
> In PECVD plasma usually occur a little high temp because mobility of
>    electrons are better as temperature higher.
>
> I think it'll possible ,if there is something to break the eletron orbit
>   from nuclear.
>
> If there is anybody to make a new process , would you join me and
>   make revolution.
>
> with thanks.
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMStaff Inc.
Harrick Plasma, Inc.
Nano-Master, Inc.