A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Ti layer measurement...
Ti layer measurement...
2009-02-09
Javier Crespo
2009-02-09
Jie Zou
2009-02-09
Evelyn B
2009-02-13
Albert Henning
2009-02-13
Brian Stahl
2009-02-13
Rick Williston
2009-02-17
Albert Henning
2009-02-18
Fei Wang
2009-02-18
Wilson, Thomas
2009-02-18
Kirt Williams
2009-02-18
Mehmet Aykol
Ti layer measurement...
Evelyn B
2009-02-09
You can pattern the metal layer by either using a lift-off process or by
etching the metal.  Once you have patterns on your wafer you can either use:

1. A profilometer   ==> a stylus runs through the wafer and detects the
difference in height between areas with metal and areas without metal.  You
can search Dektak 150 or Alpha Step profilers to get more info on how they
work.

2. Ellipsometer  ==> uses the refractive properties of the substrate and
film to determine the film thickness.  You have to check if your
ellipsometer will determine the thickness of both absorbent and
non-absorbent substrates and determine if Si is asbosbent or not.

Hope this helps.

Evelyn


On Mon, Feb 9, 2009 at 11:15 AM, Javier Crespo
wrote:

> Dear All,
>
> I want to deposit a Titanium layer to a silicon wafer by sputtering. The
> layer is about 100nm, but I don't know how to measure it. Does anyone
> know how could I measure the Ti thickness?
>
> Thanks,
>
> Xabier
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
The Branford Group
Addison Engineering