coating SiO2
Senthil Nathan Sambandam
1998-09-28
Hi

I need to deposit SiO2 layers about 10 microns thick for a microwave
device. At the moment, am using spin-on glass (solvent based) as an easy
way of getting done. However, I am not able to achieve good films beyond
4 microns.

Could anybody suggest a better speedier method to deposit SiO2 or a
better spin-on glass material.

Thanx

Senthil Nathan

______________________________________________________
Get Your Private, Free Email at http://www.hotmail.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
Process Variations in Microsystems Manufacturing
University Wafer