MEMSnet Home: MEMS-Talk: Silicon wafer thinning chemically
Silicon wafer thinning chemically
2009-03-31
Ananth Krishnan
2009-04-01
Yongliang Yang
Silicon wafer thinning chemically
Ananth Krishnan
2009-03-31
Hello,

Is there a way to chemically etch and thin down <100> oriented silicon
handle layer of a SOI wafer from 700 microns to 200 microns without
affecting the top silicon? I tried polishing, but our machine is not flat
leading to thinning down on side much more than other even after very good
alignment with respect to center of polishing lap. I need to cleave the
sample after thinning down.

--
Ananth Krishnan
Texas, USA
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
The Branford Group
Tanner EDA by Mentor Graphics