MEMSnet Home: MEMS-Talk: PR adhesion to gold
PR adhesion to gold
2009-04-13
walter
2009-04-14
Warren Dustin
PR adhesion to gold
walter
2009-04-13
Greetings all.

We are running into difficulties with the adhesion of 1813 PR to gold.
We never experienced this problem before.

In the past we used AP 100 series from Silicon resources however they no longer
seem to be in business.

We now use recommended omnicoat sold through micro chem,
I t works well.

The problem is once we develop /etch the PR, blotches of the omnicoat remain.
We cure the omnicoat at 200 degrees C.

70 percent of the wafer looks perfect the rest we cannot remove the omnicoat.
Questing what chemical can we use to remove the Omnicoat without affecting the
remaining PR pattern.

I am sure that someone has the answers out there in cyberspace.

Thanking you in advance

Zoltan
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
The Branford Group