MEMSnet Home: MEMS-Talk: Pyrex glass etching
Pyrex glass etching
2009-05-01
Terry Zhu
2009-05-04
Fei Wang
Pyrex glass etching
Terry Zhu
2009-05-01
To all,

I am trying to develop a controlled glass etching using HF/H2O. Is there any of
you who have experience about it? Any recomendations or comments about etchant
composition, temperature, stiring condition, etch rate would be appreciated.

Terry Z