RE: high precision accelerometer
Jason
1998-10-12
We build Micromachined capacitive Nickel Accelerometers.   Most of the
information you require is on our Web Site at www.silicondesigns.com  be
sure to look at the /tech.html page for some specifics on the mechanics,
etc.  If you need any more information, feel free to contact me.

--Jason Tauscher
 Senior Research Engineer
Silicon Designs, Inc.
[email protected]


-----Original Message-----
From:   Cheng-Hsien Liu [mailto:[email protected]]
Sent:   Saturday, September 26, 1998 8:40 AM
To:     [email protected]
Subject:        high precision accelerometer

Hi, MEMS colleague,

I am working on a project- high precision micromachined accelerometer using
electron tunneling transducer. I try to make a comparison table about
different
micromachined accelerometers.  If you work (or ever)on micromachined
accelerometers using any transducers (capacitive, piezoelectric,
piezoresist,..) (or know where I could find these information), could you
please email
me the following information (or point out where I could have the
information):

1. Researcher or company (references)
2. Noise floor (?mg/root(Hz) or ?micro-g/root(Hz)) (How about low
frequency?)
3. Bandwidth (?Hz)
4. Sensitivity (V/g)
5. Dynamic Range (?dB and ?g max)
6. Working principle (capacitive, tunneling, piezo....)
7. Fabrication (Bulk-micromachined, surface-micro...)
8. Proofmass (? milli-gram or ? micro-gram)
9. Device area (area including proofmass and cantilever beams or
membrane:?mmx?mm)
10. Operating Voltage (high voltage supply :V)
11. Open-Loop or closed-loop with feedback control circuit needed?
12. One axis, two axes, or three axes for each sensor unit?

The more details the better.  Your help is highly appreciated.
Best regards,


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
Mentor Graphics Corporation
MEMStaff Inc.