A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Positive sidewall, dry etch of silicon using BOSCH process
Positive sidewall, dry etch of silicon using BOSCH process
2009-05-19
shimul saha
2009-05-21
Jie Zou
2009-05-21
James Paul Grant
2009-05-21
Fei Wang
2009-05-21
[email protected]
Positive sidewall, dry etch of silicon using BOSCH process
Jie Zou
2009-05-21
Try first less bias. then less RF power. then less SF6.

On Tue, May 19, 2009 at 6:11 AM, shimul saha  wrote:
> Hello,
>
> I am using BOSCH process for deep dry etching of silicon. The gases are SF6,
O2 during etching cycles and C4F8 during deposition cycles.. At present I am
getting slightly negative sidewall, but I want a positive sidewall. Can you
please provide any hint, probably changing gas ratio (incerase or decrease any
of the gas content) or power to get a positive sidewall in etching. Any
suggestions will be greatly helpful for me. Thanking you in advance.
>
> Best regards,
> Shimul

*  Zou Jie (Jay)
*  Department of Physics
*  University of Florida
*  Tel: +1-352-846-8018
*  Email: [email protected]
*  Homepage: http://plaza.ufl.edu/zoujie/
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Addison Engineering